1.3 Tailings Consolidation Test <br />• Two samples were formed i n 2.8 i nch diameter by 1 i nch i n <br />height consolidation rings. These samples were then placed in <br />consolidometers and loaded to a maximum load of 10240 psf. The data <br />obtained in these test is presented in Appendix A. These testiwere <br />intended to determine the potential ultimate maximur~ dry density <br />which could be obtained. Values of ultimate dry density at a load <br />of 10240 psf ranged from 97.3 pcf to 99.4 pcf. <br />• <br />n <br />U <br />