• <br />• <br />,Table;Z- IIW: Pit;Atterberg;Limits and-Grain.Size Distribution;: - <br />- ,Results <br />Sample ID %M LL PI %Gravel %Sand %Fines USCS <br />2W-1 14.2 35 19 45 10 45 CL-GC <br />2W-2 12.6 30 16 55 8 37 GC <br />2W-4 11.9 25 8 31 15 54 CL <br />2W-5 8.7 24 9 75 5 20 GC <br />2W-6 12 29 14 46 7 47 CL-GC <br />2W-7 11.4 26 7 53 13 34 GC <br />IIW Avg. 11.8 28.2 12.2 50.8 9.7 39.5 - <br />Note: 2W-1 was chosen for Triaxial testing because of its <br />relatively high plasticity <br />f~ <br />